| EN AW-7075 / ISO: Al Zn5,5MgCu |
| Composition: |
Al 5.6Zn 2.5Mg 1.6Cu Cr |
| Applications: |
Aircraft and military highly stressed structural components.
Rolling stock for machine parts and tools (for rubber and plastics).
Ski poles, tennis rackets, screws and bolts, nuts.
Rivets.
Nuclear applications.
|
| Characteristic Properties: |
Heat treatable very high strength alloy with a strength slightly lower than 7010.
Very high fatigue strength.
Joining preferably by rivets, adhesives or screws.
Corrosion protection is recommended also in outdoor atmosphere.
|
| Precautions and Warnings: |
Care to be taken when selecting temper (and other thermal treatment) for balance of properties. May be clad with 7072 for better protection against stress corrosion cracking. |
| Product Forms: |
Bar, Forging, Profile section shape, Plate, Rod, Slugs impacts, Sheet, Tube, Wire
|
|