Alloys:

EN AW-1050A / ISO Al99,5

Composition: Al99.5
Alloy family: Wrought Al-Alloy
Alloy type: Non-hardenable Al-alloys
Alloy Series: Pure Al-alloys (1xxx)
Alloy Sub-series: Medium purity pure Al-alloys
Product forms available:
 Bar
 Foil
 Profile section shape
 Rod
 Slugs impacts
 Sheet
 Tube
 Wire

(Click for a list of alloys available in each form.)