Creep Rupture Properties
Wrought Alloys
Compositions
Applications
Corrosion & Anodizing
Physical & Elastic Properties
Product Forms
Formability, Machinability & weldability
Alloy Composition
Creep Properties
Fatigue Properties
Mechanical Properties
National/Company Alloy Designations
Summary
Advanced Search
------------------
Casting Alloys
Compositions
Mechanical Properties
Physical & Surface Properties
------------------
Temper Designations
Property Definitions
Alloys:
2024
3003
5052
5083
5086
5454
5754
6061
6063
6082
7075
Tempers:
T3
T4
T86
T / °C:
125
150
175
200
225
250
300
EN AW-
2024
-
T3
, 125°C
Time to Rupture,
t
/ h
Creep Rupture Stress / MPa
1000
335
3000
305
10000
270
30000
235