ATTENTION - the aluMATTER site is currently experiencing some technical problems
 
blank spacer
blank spacer
  Accueil | Plan de Site | Recherche | aluSelect | Partenaires | Au sujet de aluMATTER | Aide  
Diagrammes de Phase

Leonardo da Vinci, Helsinki Award 2006, Design and execution: Gerold Fink, Austria. Click to open PDF document about this award

Leonardo Da Vinci Helsinki Award 2006

Leonardo da Vinci, Helsinki Award 2006, Design and execution: Gerold Fink, Austria. Click to open PDF document about this award

Bronze medal for an outstanding project promoting and supporting the LifeLong Learning EU policy. Award Berlin 2007

 
Cliquez ici pour retourner à la page précédente Page 10 / 10  
Exercice: comprendre les diagrammes de phase binaire

Print out or sketch the eight binary phase diagrams found on the preceding pages. Annotate each diagram with the following information.

  1. Shade all the single phase regions.
  2. Label all the 2-phase regions.
  3. Mark the maximum solubility of the alloy element in aluminium.
  4. Mark eutectic/eutectoid points with E and mark the temperature and composition.
  5. Mark peritectic/peritectoid points with P and mark the temperature and composition.

We've done the Al-Cu diagram for you.